How to Stop Warping in 3D Printing: 7 Fixes for PLA, PETG and ABS

How to Stop Warping in 3D Printing: 7 Fixes for PLA, PETG and ABS

A big, flat print is going well, then the corners start to curl up off the bed. That is warping. Plastic shrinks as it cools, the upper layers pull inward, and the corners get levered off the build plate. These seven fixes cover the usual causes, in the order we would check them.

1. Keep the build plate clean

Finger grease is the most common reason for poor adhesion. Wash the plate with warm water and dish soap (washing-up liquid in the UK) or wipe it with isopropyl alcohol (IPA), and do not touch the print surface afterwards.

2. Set the right bed temperature

MaterialBed temperature
PLA50–60 °C (122–140 °F)
PETG70–80 °C (158–176 °F)
ABS / ASA90–110 °C (194–230 °F)

3. Add a brim or mouse ears

A brim is a thin skirt attached to the base of the part that enlarges the contact area. For delicate corners, small round discs (“mouse ears”) on the corners only are often enough. Both break off easily after printing.

4. Stop drafts

Cold air from a window, a fan or an air conditioner makes parts cool unevenly. On an open-frame printer a simple cover or enclosure helps a lot. For ABS and ASA a closed enclosure is a must.

5. Reduce the part cooling fan on the first layers

Most slicers turn the part cooling fan off for the first layers. For ABS and ASA, keep it low for the whole print.

An enclosed printer with a heated chamber makes warping far less likely:

QIDI Q2 3D Printer, 65℃ Heated Chamber and 370℃ Nozzle Unlock PPS-CF | ultra air filtration, 600mm/s high speed, AI camera, full auto leveling, 270x270x256mm build volume, unbox to print in 10 min
Show customer reviews
List Price: £429.00 You Save: £21.46 (-5%)  Price: £407.54 Buy now at Amazon* Price incl. VAT., Excl. Shipping
Last updated on November 21, 2026 at 9:13 pm - Image source: Amazon Affiliate Program. All statements without guarantee.

* Affiliate link: if you buy through it, we earn a small commission at no extra cost to you. Learn more

6. Dial in the first layer

A first layer that is too high or too fast sticks poorly. It should be pressed slightly into the plate and printed slower than the rest. Modern printers level the bed themselves, but it is still worth checking your Z offset. Our guide to the perfect first layer shows what to look for.

7. Round off sharp corners

Sharp 90-degree corners on large parts warp the most. If you design your own models, add a small radius to the outer corners. It reduces the stress noticeably.

Which printers handle warping best?

A heated, enclosed chamber is the most reliable cure, because the whole part cools slowly and evenly. That is why enclosed CoreXY printers are the usual choice for ABS and ASA, while open bed-slingers are fine for PLA and PETG with the tips above.